Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 10.0 - 15.0 % Show Supplier Material materials with Dehnung of 10.0 - 15.0 % | min., depending on the size |
Zugfestigkeit | 450.0 - 750.0 MPa Show Supplier Material materials with Zugfestigkeit of 450.0 - 750.0 MPa | depending on the size |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Parts and accessories for heat treatment furnace and quenching baths. Solenoid valve components. | |
Other | Available products: Other products: contact the supplier |