Description

Martensitic grade combining high mechanical properties with good corrosion resistance on suitably polished surfaces in moderately aggressive non-chlorinated environments (optimum in treated state) Good resistance in oxidizing atmosphere up to 600°C. UGIMAR grade produced according to an Ugitech process to significantly improve its machinability (15% to 25% increase in productivity), up to diameter 115 mm

Related Standards

Equivalent Materials

Diese Materialdaten wurden von Ugitech SA zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Chemical properties

PropertyValueComment

Chrom

12.5 %

Show Supplier Material materials with Chrom of 12.5 %

Kohlenstoff

0.12 %

Show Supplier Material materials with Kohlenstoff of 0.12 %

Schwefel

0.03

Show Supplier Material materials with Schwefel of 0.03

max.

Technological properties

Property
Application areas

Mechanical engineering, oil and petrochemicals industry, food and food processing industry, decoration and household appliances, transport and cutlery: shafts, pistons, liners, valves, nuts and bolts, etc.

Corrosion properties

Atmospheres, fresh waters (check water analysis). Oxidizing saline solutions free of chlorides, fluorides, iodides, bromides, etc. Cold diluted nitric solutions. Certain cold diluted organic acids: picric, tannic, lactic, etc. Non-corrosive products such as: alcohol, benzol, petroleum, oil, soap, etc.

Heat Treatment

Tempering curves on the right side of the material page.

Tempering temperature: Indicative mechanical properties after quenching in oil at 950°C and tempering for 2 hours.

Other

Available products:


ProductShapeFinishToleranceDimensions
BarRoundRolled and descaled bars12 to 1322 to 15 mm
RoundTurned and polished9 to 1122 to 115 mm
RoundDrawn bar8 to 93 to 55 mm
RoundGround bar6 to 93 to 80 mm
HexagonalDrawn bar113 to 55 mm
Wire rodRoundPickled5.0 to 32 mm
Drawn wireRound16.0 to 1.0 mm


Other products: contact the supplier

Surface Treatment

Pickling: please consult the supplier first.