Allgemein
Property | Value |
---|---|
Dichte | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 10 % Show Supplier Material materials with Dehnung of 10 % | min. |
Elastizitätsmodul | 220 GPa Show Supplier Material materials with Elastizitätsmodul of 220 GPa | |
Zugfestigkeit | 550.0 - 800.0 MPa Show Supplier Material materials with Zugfestigkeit of 550.0 - 800.0 MPa |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0000111 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0000111 1/K | 20 to 100°C |
Wärmeleitfähigkeit | 15 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 6.100000000000001e-07 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.100000000000001e-07 Ω·m |
Magnetisch
Property | Value | Comment |
---|---|---|
Koerzitivfeldstärke | 300.0 - 400.0 A/m Show Supplier Material materials with Koerzitivfeldstärke of 300.0 - 400.0 A/m | Drawn bar with magnetic annealing and >600 only drawn. |
Relative magnetische Permeabilität | 900 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 900 [-] | Drawn bar with magnetic annealing and <500 only drawn. |
1100 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1100 [-] | Drawn bar with magnetic annealing and <500 only drawn. | |
Remanenz | 0.8 - 1.0 T Show Supplier Material materials with Remanenz of 0.8 - 1.0 T | Drawn bar with magnetic annealing and 0.6-0.8 only drawn. |
Sättigungspolarisation | 1.57 T Show Supplier Material materials with Sättigungspolarisation of 1.57 T | Drawn bar with magnetic annealing |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.5 - 18.5 % Show Supplier Material materials with Chrom of 17.5 - 18.5 % | |
Kohlenstoff | 0.08 Show Supplier Material materials with Kohlenstoff of 0.08 | max. |
Mangan | 1.0 Show Supplier Material materials with Mangan of 1.0 | max. |
Molybdän | 1.5 - 2.5 % Show Supplier Material materials with Molybdän of 1.5 - 2.5 % | |
Phosphor | 0.04 Show Supplier Material materials with Phosphor of 0.04 | max. |
Schwefel | 0.15 - 0.25 % Show Supplier Material materials with Schwefel of 0.15 - 0.25 % | max. |
Silizium | 1.0 Show Supplier Material materials with Silizium of 1.0 | max. |
Stickstoff | 0.07 Show Supplier Material materials with Stickstoff of 0.07 | max. |
Technological properties
Property | ||
---|---|---|
Application areas | ||
Corrosion properties | Generalized corrosion in 2M sulphuric acid and at ambient temperature. Good resistance to generalized corrosion in sulphuric acid, better than that of UGI®4105. | |
General machinability | Turning: UGI® 4114 has very good turning machinability (better than that of UGI® 4305). | |
Heat Treatment | Softening: Maximum softening heat treatment with holding temperature of 800°C followed by air cooling. Do not exceed 825°C. | |
Hot forming | Forging: Heated slowly to 850°C, then more quickly to 1100/1130°C. Forging between 1130°C and 750°C. | |
Other | Available products: Contact the supplier for dimensions | |
Surface Treatment | contact the supplier |