Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | min. | |
Elastizitätsmodul | 20 °C | 200 GPa Show Supplier Material materials with Elastizitätsmodul of 200 GPa | |
100 °C | 194 GPa Show Supplier Material materials with Elastizitätsmodul of 194 GPa | ||
200 °C | 183 GPa Show Supplier Material materials with Elastizitätsmodul of 183 GPa | ||
Zugfestigkeit | 600 MPa Show Supplier Material materials with Zugfestigkeit of 600 MPa | max. |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0000165 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0000165 1/K | 20 to 100°C | |
0.0000175 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0000175 1/K | 20 to 200°C | ||
Max. Betriebstemperatur | 250.0 °C Show Supplier Material materials with Max. Betriebstemperatur of 250.0 °C | ||
Spezifische Wärmekapazität | 500 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | ||
Wärmeleitfähigkeit | 20 °C | 15 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15 W/(m·K) | |
100 °C | 16 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 16 W/(m·K) | ||
250 °C | 18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 18 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20 °C | 0.00000078 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.00000078 Ω·m |
100 °C | 0.00000083 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.00000083 Ω·m | |
250 °C | 0.00000090 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.00000090 Ω·m |
Magnetisch
Property | Value |
---|---|
Relative magnetische Permeabilität | 1.02 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.02 [-] |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16.0 - 19.0 % Show Supplier Material materials with Chrom of 16.0 - 19.0 % | |
Kohlenstoff | 0.05 - 0.15 % Show Supplier Material materials with Kohlenstoff of 0.05 - 0.15 % | |
Mangan | 2.0 Show Supplier Material materials with Mangan of 2.0 | max. |
Molybdän | 0.8 Show Supplier Material materials with Molybdän of 0.8 | max. |
Nickel | 6.0 - 9.5 % Show Supplier Material materials with Nickel of 6.0 - 9.5 % | |
Phosphor | 0.045 Show Supplier Material materials with Phosphor of 0.045 | max. |
Schwefel | 0.015 Show Supplier Material materials with Schwefel of 0.015 | max. |
Silizium | 1.0 Show Supplier Material materials with Silizium of 1.0 | max. |
Stickstoff | 0.11 Show Supplier Material materials with Stickstoff of 0.11 | max. |
Technological properties
Property | ||
---|---|---|
Application areas | ||
Cold Forming | Drawing – Profiling Like all high-carbon grade austenitic steels, UGI® S302 is hardened significantly during cold transformation. However, it has good ductility, with a potential reduction in cross section of up to 90% or more. | |
Corrosion properties | UGI® S302 has good corrosion resistance in moderately corrosive environments. It is widely used in humid or aqueous environments with a limited chloride content. The use of UGI® S302 in marine environments should be avoided, especially in its drawn spring-wire version. | |
Heat Treatment | Springs' mechanical strength can be increased up to 250 Mpa (depending on the diameter) by heat treatment performed on the springs. The Rp0.2/Rm ratio can increase by 5% after such a treatment. Static treatment: Static treatment temp.: 350/425°C, Recommended duration 0.5 to 4 hours depending on batch size Treatment in continuous oven: Heat treatment temp.: 25°C higher than in, Min. treatment duration: 3 minutes | |
Hot forming | UGI® S302 has good hot forgeability. Forging temperatures are between 900°C and 1100°C. Once forged, the parts must be cooled swiftly, i.e. chilled in water to avoid problems of sensitization of the grade to poten-tial grain-boundary corrosion | |
Other | Available products: Other: please consult the supplier |