Das Material: 'Linear Low Density Polyethylene (LLD PE) Chalk Batch for Film Applications', nach dem Sie gesucht haben, wurde durch das untenstehende ersetzt.

G-3645UV (LLDPE)

Alternative und Handelsbezeichungen
G-3645UV (LLDPE)
Want to keep this datasheet? Save it now in your required format

Description

GREENETHENE G-3645UV is a Low Density Linear Polyethylene Resin (LLDPE) in powder form, additivated with antioxidants and UV stabilizers. It is suitable for Rotational Molding applications. Items produced by GREENETHENE G-3645UV have a very good balance between mechanical properties and ESCR resistance. G-3645UV is produced in: natural, black, terracotta, fire red, yellow & blue. GREENETHENE G-3645UV meets the requirement stipulated in standard IS:10141:2001 on “Specification for Polyethylene for safe use in contact with foodstuff, pharmaceuticals & Drinking Water”. It also conforms to IS 12701:1996 –“Specification For Rotational Moulded Polyethylene Water Storage Tanks.”.

Diese Materialdaten wurden von GreenAge Industries zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

0.94 g/cm³

Show Supplier Material materials with Dichte of 0.94 g/cm³

ASTM D1505

Mechanisch

PropertyTemperatureValueComment

Biegemodul

23.0 °C

0.23 - 0.59 GPa

Show Supplier Material materials with Biegemodul of 0.23 - 0.59 GPa

ASTM D790

Dehnung

23.0 °C

165 - 600 %

Show Supplier Material materials with Dehnung of 165 - 600 %

ASTM D638

Härte, Shore D

23.0 °C

55 [-]

Show Supplier Material materials with Härte, Shore D of 55 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

250 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250 J/m

ASTM D256

Streckgrenze

23.0 °C

17.5 - 18 MPa

Show Supplier Material materials with Streckgrenze of 17.5 - 18 MPa

ASTM D638

Zugfestigkeit

23.0 °C

11.75 MPa

Show Supplier Material materials with Zugfestigkeit of 11.75 MPa

ASTM D638

Thermisch

PropertyValueComment

Vicat-Erweichungstemperatur

117 °C

Show Supplier Material materials with Vicat-Erweichungstemperatur of 117 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Schmelzmassenflussrate

4.5 g/10min

Show Supplier Material materials with Schmelzmassenflussrate of 4.5 g/10min

ASTM D1238, 190°C/2.16kg

Technological properties

Property
Application areas

Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3645UV is suggested for the production of wide variety of Storage tank applications of water, chemicals & Oils. GREENETHENE G-3645UV can also be used for off-shore flotation buoys and road crash barriers.

Certifications

List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996

Color

Natural, black, terracotta, fire red, yellow and blue.

Processing methods

Compression molded & rotomolded