Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.57 g/cm³ Show Material materials with Dichte of 6.57 g/cm³ | Typical for Zirconium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 68 GPa Show Material materials with Elastizitätsmodul of 68 GPa | Typical for Zirconium |
Härte, Brinell | 20.0 °C | 235 [-] Show Material materials with Härte, Brinell of 235 [-] | |
Härte, Rockwell B | 20.0 °C | 99 [-] Show Material materials with Härte, Rockwell B of 99 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Zirconium |
Schubmodule | 23.0 °C | 35 GPa Show Material materials with Schubmodule of 35 GPa | Typical for Zirconium |
Streckgrenze Rp 0,2 | 20.0 °C | 276 MPa Show Material materials with Streckgrenze Rp 0,2 of 276 MPa | |
Zugfestigkeit | 20.0 °C | 413 MPa Show Material materials with Zugfestigkeit of 413 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Schmelzpunkt | 1845 °C Show Material materials with Schmelzpunkt of 1845 °C | Typical for Zirconium | |
Spezifische Wärmekapazität | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 281 - 289 J/(kg·K) | Typical for Zirconium |
Wärmeleitfähigkeit | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19 - 27 W/(m·K) | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Hafnium | 4.5 % Show Material materials with Hafnium of 4.5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Sauerstoff | 0.3 % Show Material materials with Sauerstoff of 0.3 % |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % |
Wasserstoff | 5E-3 % Show Material materials with Wasserstoff of 5E-3 % |
Zinn | 1 - 2 % Show Material materials with Zinn of 1 - 2 % |