Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Austenitischer rostfreier Stahl
ASTM A276 Grade S20910 AnnealedWrought Copper Bronze Aluminium Bronze
NC4 - CuAl10Ni5Fe4 - C63000 / C63200Geliefert von:
Lebronze AlloysFerritischer Edelstahl
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Nickel Chromium Alloy
DIN 17742 Grade NiCr15Fe soft annealed (+A)Austenitischer rostfreier Stahl
EN 10095 Grade X15CrNiSi25-4 solution annealed (+AT)Wrought Copper Nickel Grade
NIBRON SPECIAL® Copper AlloyWrought Copper High Copper Alloy
EN 1652 Grade CuCo2Be THFerritischer Edelstahl
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10277-4 Grade C15R soft annealed and cold drawn (+A+C)Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 TH