DIN 1725-1 Grade 3.3315 O

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

The AlMg alloy is characterised all by a good corrosion resistance. It is sea water steady and resistant to saline atmosphere. The Mg content increase the strength, the cold forming capacity decreases with it. The alloys of this type are nature hard, i.e. only by a cold forming and not by a purposeful heat treatment a strength increase can be attained. The material is well polishabel and anodisable. The splinter-giving machinability becomes better with increasing Mg content just like the weldability. The alloy AlMg1 reaches strength grades to F 22. Application: Their main field of application is the building industry. In the building industry for claddings, roofing and trim, for transport containers. For metal goods, like building fittings, table-ware, flow pressed parts, reflectors. In food industry, for furniture (incl. camping furniture) as well as for describe and for covers with composite slabs (intermediate layer: Polyethylene).

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.69 g/cm³

Show Material materials with Dichte of 2.69 g/cm³

O

EN 573-3, EN 485, EN 754, EN 755

20.0 °C

2.69 g/cm³

Show Material materials with Dichte of 2.69 g/cm³

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Biegewinkel 180°

0.5 °/t

Show Material materials with Biegewinkel 180° of 0.5 °/t

O

EN 573-3, EN 485

1.0 °/t

Show Material materials with Biegewinkel 180° of 1.0 °/t

O

EN 573-3, EN 485

Biegewinkel 90°

1.0 °/t

Show Material materials with Biegewinkel 90° of 1.0 °/t

O

EN 573-3, EN 485

1.5 °/t

Show Material materials with Biegewinkel 90° of 1.5 °/t

O

EN 573-3, EN 485

Dehnung

15.0 %

Show Material materials with Dehnung of 15.0 %

O

EN 573-3, EN 485

A50

16.0 %

Show Material materials with Dehnung of 16.0 %

O

EN 573-3, EN 754

A50

18.0 %

Show Material materials with Dehnung of 18.0 %

O

EN 573-3, EN 754

A100

18.0 %

Show Material materials with Dehnung of 18.0 %

O

EN 573-3, EN 755

A50

19.0 %

Show Material materials with Dehnung of 19.0 %

O

EN 573-3, EN 485

A50

20.0 %

Show Material materials with Dehnung of 20.0 %

O

EN 573-3, EN 485, EN 755

A100

20.0 %

Show Material materials with Dehnung of 20.0 %

O

EN 573-3, EN 485

A50

22.0 %

Show Material materials with Dehnung of 22.0 %

O

EN 573-3, EN 485

A50

24.0 %

Show Material materials with Dehnung of 24.0 %

O

EN 573-3, EN 485

A50

20.0 °C

13.0 %

Show Material materials with Dehnung of 13.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

14.0 %

Show Material materials with Dehnung of 14.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Wire

A100

20.0 °C

16.0 %

Show Material materials with Dehnung of 16.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Wire

A10

20.0 °C

18.0 %

Show Material materials with Dehnung of 18.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Tube

A10

20.0 °C

18.0 %

Show Material materials with Dehnung of 18.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod

20.0 °C

20.0 %

Show Material materials with Dehnung of 20.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

20.0 %

Show Material materials with Dehnung of 20.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Tube

20.0 °C

21.0 %

Show Material materials with Dehnung of 21.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

A10

20.0 °C

24.0 %

Show Material materials with Dehnung of 24.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Elastizitätsmodul

69.5 GPa

Show Material materials with Elastizitätsmodul of 69.5 GPa

O

EN 573-3, EN 485, EN 754, EN 755

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastizitätsmodul of 60.0 - 65.0 GPa

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

Härte, Brinell

29.0 [-]

Show Material materials with Härte, Brinell of 29.0 [-]

O

EN 573-3, EN 485

20.0 °C

30.0 [-]

Show Material materials with Härte, Brinell of 30.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Tube, Wire

20.0 °C

32.0 [-]

Show Material materials with Härte, Brinell of 32.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Schubmodule

26.1 GPa

Show Material materials with Schubmodule of 26.1 GPa

O

EN 573-3, EN 485, EN 754, EN 755

20.0 °C

25.0 GPa

Show Material materials with Schubmodule of 25.0 GPa

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

Zugfestigkeit

100.0 - 145.0 MPa

Show Material materials with Zugfestigkeit of 100.0 - 145.0 MPa

O

EN 573-3, EN 485, EN 754

100.0 - 150.0 MPa

Show Material materials with Zugfestigkeit of 100.0 - 150.0 MPa

O

EN 573-3, EN 755

20.0 °C

100.0 MPa

Show Material materials with Zugfestigkeit of 100.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Tube, Wire

20.0 °C

105.0 - 140.0 MPa

Show Material materials with Zugfestigkeit of 105.0 - 140.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

20.0 °C

105.0 - 135.0 MPa

Show Material materials with Zugfestigkeit of 105.0 - 135.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

-50 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

-50.0 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

20 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

20 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

20 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

20 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

100 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

100.0 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

200 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

200.0 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

300 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

300.0 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

O

EN 573-3, EN 485, EN 754, EN 755, DIN 1725-1, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

Max. Betriebstemperatur

150.0 °C

Show Material materials with Max. Betriebstemperatur of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Schmelzpunkt

630.0 - 650.0 °C

Show Material materials with Schmelzpunkt of 630.0 - 650.0 °C

O

EN 573-3, EN 485, EN 754, EN 755

Spezifische Wärmekapazität

20.0 °C

879.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 879.0 J/(kg·K)

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

Wärmeleitfähigkeit

20.0 °C

160.0 - 220.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 160.0 - 220.0 W/(m·K)

O

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Rod, Sheet, Flat, Strip, Tube, Wire

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

20.0 °C

23000000.0 - 31000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 31000000.0 S/m

O

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Rod, Sheet, Flat, Strip, Tube, Wire

spezifischer Widerstand

3.23e-08 - 4.35e-08 Ω·m

Show Material materials with spezifischer Widerstand of 3.23e-08 - 4.35e-08 Ω·m

O

EN 573-3, EN 485, EN 754, EN 755

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.1 %

Show Material materials with Chrom of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Rod, Sheet, Flat, Strip, Tube, Wire

Eisen

0.45 %

Show Material materials with Eisen of 0.45 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

0.70 %

Show Material materials with Eisen of 0.70 %

O

EN 573-3, EN 485, EN 754, EN 755

Kupfer

0.05 %

Show Material materials with Kupfer of 0.05 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

0.2 %

Show Material materials with Kupfer of 0.2 %

O

EN 573-3, EN 485, EN 754, EN 755

Magnesium

0.7 - 1.1 %

Show Material materials with Magnesium of 0.7 - 1.1 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

1.1 - 1.8 %

Show Material materials with Magnesium of 1.1 - 1.8 %

O

EN 573-3, EN 485, EN 754, EN 755

Mangan

0.15 %

Show Material materials with Mangan of 0.15 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

0.3 %

Show Material materials with Mangan of 0.3 %

O

EN 573-3, EN 485, EN 754, EN 755

Silizium

0.3 %

Show Material materials with Silizium of 0.3 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

0.4 %

Show Material materials with Silizium of 0.4 %

O

EN 573-3, EN 485, EN 754, EN 755

Zink

0.2 %

Show Material materials with Zink of 0.2 %

O

DIN 1725-1, EN 573-3, EN 573-4

Rod, Sheet, Flat, Strip, Tube, Wire

0.25 %

Show Material materials with Zink of 0.25 %

O

EN 573-3, EN 485, EN 754, EN 755

Technological properties

Property
Workability

Good workability.