DIN 1725-1 Grade 3.3315 H28

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

The AlMg alloy is characterised all by a good corrosion resistance. It is sea water steady and resistant to saline atmosphere. The Mg content increase the strength, the cold forming capacity decreases with it. The alloys of this type are nature hard, i.e. only by a cold forming and not by a purposeful heat treatment a strength increase can be attained. The material is well polishabel and anodisable. The splinter-giving machinability becomes better with increasing Mg content just like the weldability. The alloy AlMg1 reaches strength grades to F 22. Application: Their main field of application is the building industry. In the building industry for claddings, roofing and trim, for transport containers. For metal goods, like building fittings, table-ware, flow pressed parts, reflectors. In food industry, for furniture (incl. camping furniture) as well as for describe and for covers with composite slabs (intermediate layer: Polyethylene).

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.69 g/cm³

Show Material materials with Dichte of 2.69 g/cm³

H28

EN 573-3, EN 485

20.0 °C

2.69 g/cm³

Show Material materials with Dichte of 2.69 g/cm³

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Biegewinkel 90°

1.5 °/t

Show Material materials with Biegewinkel 90° of 1.5 °/t

H28

EN 573-3, EN 485

2.5 °/t

Show Material materials with Biegewinkel 90° of 2.5 °/t

H28

EN 573-3, EN 485

3.0 °/t

Show Material materials with Biegewinkel 90° of 3.0 °/t

H28

EN 573-3, EN 485

Dehnung

1.0 %

Show Material materials with Dehnung of 1.0 %

H28

EN 573-3, EN 485

A50

2.0 %

Show Material materials with Dehnung of 2.0 %

H28

EN 573-3, EN 485

A50

3.0 %

Show Material materials with Dehnung of 3.0 %

H28

EN 573-3, EN 485

A50

20.0 °C

4.0 %

Show Material materials with Dehnung of 4.0 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

A10

20.0 °C

5.0 %

Show Material materials with Dehnung of 5.0 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Elastizitätsmodul

69.5 GPa

Show Material materials with Elastizitätsmodul of 69.5 GPa

H28

EN 573-3, EN 485

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastizitätsmodul of 60.0 - 65.0 GPa

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Härte, Brinell

58.0 [-]

Show Material materials with Härte, Brinell of 58.0 [-]

H28

EN 573-3, EN 485

20.0 °C

57.0 [-]

Show Material materials with Härte, Brinell of 57.0 [-]

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Schubmodule

26.1 GPa

Show Material materials with Schubmodule of 26.1 GPa

H28

EN 573-3, EN 485

20.0 °C

25.0 GPa

Show Material materials with Schubmodule of 25.0 GPa

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Zugfestigkeit

185.0 MPa

Show Material materials with Zugfestigkeit of 185.0 MPa

H28

EN 573-3, EN 485

20.0 °C

190.0 MPa

Show Material materials with Zugfestigkeit of 190.0 MPa

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

-50 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

-50.0 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

20 °C

2.18e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

20 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

20 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

20 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

100 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

100.0 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

200 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

200.0 °C

2.45e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

300 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

300.0 °C

2.55e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K

H28

EN 573-3, EN 485, DIN 1725-1, EN 573-4

Sheet

Max. Betriebstemperatur

150.0 °C

Show Material materials with Max. Betriebstemperatur of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Schmelzpunkt

630.0 - 650.0 °C

Show Material materials with Schmelzpunkt of 630.0 - 650.0 °C

H28

EN 573-3, EN 485

Spezifische Wärmekapazität

20.0 °C

879.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 879.0 J/(kg·K)

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

Wärmeleitfähigkeit

20.0 °C

160.0 - 220.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 160.0 - 220.0 W/(m·K)

H28

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Sheet

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

20.0 °C

23000000.0 - 31000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 31000000.0 S/m

H28

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Sheet

spezifischer Widerstand

3.23e-08 - 4.35e-08 Ω·m

Show Material materials with spezifischer Widerstand of 3.23e-08 - 4.35e-08 Ω·m

H28

EN 573-3, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.1 %

Show Material materials with Chrom of 0.1 %

H28

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Sheet

Eisen

0.45 %

Show Material materials with Eisen of 0.45 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

0.70 %

Show Material materials with Eisen of 0.70 %

H28

EN 573-3, EN 485

Kupfer

0.05 %

Show Material materials with Kupfer of 0.05 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

0.2 %

Show Material materials with Kupfer of 0.2 %

H28

EN 573-3, EN 485

Magnesium

0.7 - 1.1 %

Show Material materials with Magnesium of 0.7 - 1.1 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

1.1 - 1.8 %

Show Material materials with Magnesium of 1.1 - 1.8 %

H28

EN 573-3, EN 485

Mangan

0.15 %

Show Material materials with Mangan of 0.15 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

0.3 %

Show Material materials with Mangan of 0.3 %

H28

EN 573-3, EN 485

Silizium

0.3 %

Show Material materials with Silizium of 0.3 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

0.4 %

Show Material materials with Silizium of 0.4 %

H28

EN 573-3, EN 485

Zink

0.2 %

Show Material materials with Zink of 0.2 %

H28

DIN 1725-1, EN 573-3, EN 573-4

Sheet

0.25 %

Show Material materials with Zink of 0.25 %

H28

EN 573-3, EN 485

Technological properties

Property
Workability

Good workability.