Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 20.0 °C | 2.78 g/cm³ Show Material materials with Dichte of 2.78 g/cm³ | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 20.0 °C | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Härte, Brinell | 20.0 °C | 125.0 [-] Show Material materials with Härte, Brinell of 125.0 [-] | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 27.5 GPa Show Material materials with Schubmodule of 27.5 GPa | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Zugfestigkeit | 20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium | ||||
Schmelzpunkt | 465.0 - 655.0 °C Show Material materials with Schmelzpunkt of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium | ||||
Spezifische Wärmekapazität | 795.0 - 1050.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium | ||||
Wärmeleitfähigkeit | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 160.0 W/(m·K) | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 19000000.0 - 23000000.0 S/m | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
spezifischer Widerstand | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 - 0.3 % Show Material materials with Chrom of 0.1 - 0.3 % | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Eisen | 0.5 Show Material materials with Eisen of 0.5 | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Kupfer | 0.5 - 1.0 % Show Material materials with Kupfer of 0.5 - 1.0 % | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Magnesium | 2.6 - 3.7 % Show Material materials with Magnesium of 2.6 - 3.7 % | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Mangan | 0.1 - 0.4 % Show Material materials with Mangan of 0.1 - 0.4 % | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Silizium | 0.5 Show Material materials with Silizium of 0.5 | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Zink | 4.3 - 5.2 % Show Material materials with Zink of 4.3 - 5.2 % | T5 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |