Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 20.0 °C | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Rod, Plate | Transverse |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Rod, Plate | ||
Elastizitätsmodul | 20.0 °C | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod | |
Härte, Brinell | 20.0 °C | 140.0 [-] Show Material materials with Härte, Brinell of 140.0 [-] | T651 | WL 3.4364-1, DIN 1725-1 | Rod, Plate | Transverse |
20.0 °C | 140.0 [-] Show Material materials with Härte, Brinell of 140.0 [-] | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 150.0 [-] Show Material materials with Härte, Brinell of 150.0 [-] | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 150.0 [-] Show Material materials with Härte, Brinell of 150.0 [-] | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
Kompressionsmodul | 20.0 °C | 72.5 GPa Show Material materials with Kompressionsmodul of 72.5 GPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod | |
Plane-Strain Fracture Toughnes | 20.0 °C | 19.6 - 29.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 19.6 - 29.0 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | |
20.0 °C | 19.6 - 24.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 19.6 - 24.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 19.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 19.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 21.5 - 36.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 21.5 - 36.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 21.5 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 21.5 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 21.5 - 22.1 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 21.5 - 22.1 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 22.1 - 36.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.1 - 36.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 22.1 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.1 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
20.0 °C | 24.6 - 29.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 24.6 - 29.0 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 24.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 24.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 29.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 29.0 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 36.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 36.6 MPa·√m | T651 | WL 3.4364-1, DIN 1725-1 | Rod | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Schubmodule | 26.4 - 27.1 GPa Show Material materials with Schubmodule of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 430.0 MPa Show Material materials with Zugfestigkeit of 430.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse |
20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 480.0 MPa Show Material materials with Zugfestigkeit of 480.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod | Transverse | |
20.0 °C | 490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 520.0 MPa Show Material materials with Zugfestigkeit of 520.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Rod, Plate | Transverse | |
20.0 °C | 520.0 MPa Show Material materials with Zugfestigkeit of 520.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | ||
20.0 °C | 530.0 MPa Show Material materials with Zugfestigkeit of 530.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Plate | Transverse | |
20.0 °C | 530.0 MPa Show Material materials with Zugfestigkeit of 530.0 MPa | T651 | WL 3.4364-1, DIN 1725-1 | Rod, Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Schmelzpunkt | 465.0 - 655.0 °C Show Material materials with Schmelzpunkt of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Spezifische Wärmekapazität | 795.0 - 1050.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Wärmeleitfähigkeit | 121.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.18 - 0.28 % Show Material materials with Chrom of 0.18 - 0.28 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Eisen | 0.5 Show Material materials with Eisen of 0.5 | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Kupfer | 1.2 - 2.0 % Show Material materials with Kupfer of 1.2 - 2.0 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Magnesium | 2.1 - 2.9 % Show Material materials with Magnesium of 2.1 - 2.9 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Mangan | 0.3 Show Material materials with Mangan of 0.3 | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Silizium | 0.4 Show Material materials with Silizium of 0.4 | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Titan | 0.2 Show Material materials with Titan of 0.2 | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Zink | 5.1 - 6.1 % Show Material materials with Zink of 5.1 - 6.1 % | T651 | WL 3.4364-1, DIN 1725-1 | Plate, Rod |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |