Allgemein
Abmessung
Property | Value |
---|---|
Breite | 1540 mm Show Supplier Material materials with Breite of 1540 mm |
Dimensions | Standard stock sizes: 1540mm x 3048mm and 20-570mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 2.5 - 4.5 % Show Supplier Material materials with Dehnung A5 of 2.5 - 4.5 % | |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa | |
Härte, HBW | 23.0 °C | 110 - 120 [-] Show Supplier Material materials with Härte, HBW of 110 - 120 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 290 - 340 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 290 - 340 MPa | |
Zugfestigkeit | 23.0 °C | 320 - 380 MPa Show Supplier Material materials with Zugfestigkeit of 320 - 380 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 875 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 125 - 155 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 125 - 155 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.10E+7 - 2.40E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.10E+7 - 2.40E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T79, solution heat treated and artificially aged |