Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Dichte of 2.66 g/cm³ |
Oberflächenrauigkeit | 15 μm Show Supplier Material materials with Oberflächenrauigkeit of 15 μm |
Abmessung
Property | Value |
---|---|
Breite | 1520 mm Show Supplier Material materials with Breite of 1520 mm |
Dimensions | Standard stock sizes: 1520mm x 3020mm, 1570mm x 3670mm, 2160mm x 4000mm and 20-1070mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 10 - 15 % Show Supplier Material materials with Dehnung A5 of 10 - 15 % | |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa | |
Härte, HBW | 23.0 °C | 68 - 75 [-] Show Supplier Material materials with Härte, HBW of 68 - 75 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 110 - 130 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 110 - 130 MPa | |
Zugfestigkeit | 23.0 °C | 230 - 290 MPa Show Supplier Material materials with Zugfestigkeit of 230 - 290 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.33E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 900 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 110 - 130 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 110 - 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.60E+7 - 1.80E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: O3, homogenized and stress relieved |