General
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 900.0 % Show Supplier Material materials with Elongation of 900.0 % | ASTM D412 |
Hardness, Shore A | 75.0 [-] Show Supplier Material materials with Hardness, Shore A of 75.0 [-] | ASTM D2240 |
Tear strength | 110.0 kN/m Show Supplier Material materials with Tear strength of 110.0 kN/m | ASTM D624 |
Tensile strength | 19.0 MPa Show Supplier Material materials with Tensile strength of 19.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |