Acero de alto carbono
DIN 17222 Grade Ck101 cold rolled and soft annealed (+C+A)Acero de alto carbono
EN 10270-1 Grade DH patented cold drawnAcero de alto carbono
EN 10270-1 Grade DM patented cold drawnAcero de alto carbono
EN 10270-1 Grade SH patented cold drawnAcero de alto carbono
DIN 17223-1 Grade D patented cold drawnAcero de alto carbono
EN 10132-4 Grade C100S soft annealed or soft annealed and skin passed (+A or +A+LC)Acero de alto carbono
EN 10270-1 Grade SL patented cold drawnAcero de alto carbono
EN 10270-1 Grade SM patented cold drawnAcero para herramientas y maquinaria
EN 10132-4 Grade 102Cr6 soft annealed or soft annealed and skin passed (+A or +A+LC)Acero de alto carbono
EN 10132-4 Grade C100S quenched and tempered (+QT)Acero de alto carbono
EN 10132-4 Grade C100S cold rolled (+CR)Acero de alto carbono
EN 10132-4 Grade C100S quenched (+Q)Acero para herramientas y maquinaria
EN 10132-4 Grade 102Cr6 quenched and tempered (+QT)Acero para herramientas y maquinaria
EN 10132-4 Grade 102Cr6 quenched (+Q)Acero inoxidable martensítico
SEW 410 Grade G-X120Cr29 cast conditionAcero inoxidable ferrítico
SEW 410 Grade G-X120CrMo29-2 cast conditionAcero inoxidable martensítico
SEW 400 Grade X105CrMo17 soft annealed (+A)Acero de alto carbono
DIN 17230 Grade 100Cr2 annealed to achieve spheroidized carbides (+AC)