Coefficient of friction: 0.47 [-]

Quick Comparison

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFL36

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ THERMOCOMP™ Compound OF008

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFL369

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL14

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OCP36 - Asia

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OCP36 - Americas

Suministrada por:

Sabic

Polyamide 12 (PA12)

LNP™ LUBRICOMP™ Compound SCP36

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL24

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL36XXY

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL42

Suministrada por:

Sabic

Éter de polifenileno (PPE)

LNP™ LUBRICOMP™ Compound ZFL34

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFI14

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RBL36XXJ

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL34EH

Suministrada por:

Sabic

Poliéter éter cetona (PEEK)

LNP™ LUBRICOMP™ Compound LX00430

Suministrada por:

Sabic

Polyvinylidenefluoride (PVDF)

LNP™ LUBRICOMP™ Compound 5CL23

Suministrada por:

Sabic

Polisulfona (PSU)

LNP™ LUBRICOMP™ Compound GFL36L

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL36EU

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL34

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL36P

Suministrada por:

Sabic
Página 1 de 4