Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R390Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R470Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R540Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R600Leaded Brass
EN 12167 Grade CuZn43Pb2 H110Leaded Brass
EN 12167 Grade CuZn43Pb2 H130Leaded Brass
EN 12167 Grade CuZn43Pb2 R430Leaded Brass
EN 12167 Grade CuZn43Pb2 R480Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R700Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 H090Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 H120Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 H170Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 H190Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 H220Leaded Brass
EN 12167 Grade CuZn43Pb2 M