Cobre: 56 %

Quick Comparison

Cast Copper Brass Yellow Brass

ASTM B505 Grade C86500

Suministrada por:

1 proveedor Matmatch

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86400

Suministrada por:

1 proveedor Matmatch

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86700

Suministrada por:

1 proveedor Matmatch

Wrought Copper Nickel Silver Grade

EN 12164 Grade CuNi12Zn30Pb1 R420

Wrought Copper Nickel Silver Grade

EN 1652 Grade CuNi18Zn27 R390

Wrought Copper Nickel Silver Grade

EN 1652 Grade CuNi18Zn27 R470

Wrought Copper Nickel Silver Grade

EN 1652 Grade CuNi18Zn27 R540

Wrought Copper Nickel Silver Grade

EN 1652 Grade CuNi18Zn27 R600

Wrought Copper Nickel Silver Grade

EN 12164 Grade CuNi12Zn30Pb1 R650

Wrought Copper Nickel Silver Grade

EN 12167 Grade CuNi12Zn30Pb1 R430

Wrought Copper Nickel Silver Grade

EN 12167 Grade CuNi12Zn30Pb1 R480

Wrought Copper Nickel Silver Grade

EN 12166 Grade CuNi12Zn30Pb1 H110

Wrought Copper Nickel Silver Grade

EN 12166 Grade CuNi12Zn30Pb1 H130

Wrought Copper Nickel Silver Grade

EN 1652 Grade CuNi18Zn27 R700

Wrought Copper Nickel Silver Grade

EN 12166 Grade CuNi12Zn30Pb1 H02
Página 1 de 10