Rigidez dieléctrica: 60 kV/mm

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-07

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-04

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 PC

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 WR

Suministrada por:

Arkema: High Performance Polymers

Polytetrafluoroethylene (PTFE)

3M™ Dyneon™ (PTFE Granules TF 1641)