3M™ Dyneon™ (PTFE Granules TF 1641)

Want to keep this datasheet? Save it now in your required format

Description

Free-flowing suspension PTFE for general moulding applications like seals, shaped parts and automatically or isostatically moulded articles.


Special Features are:

  • Meets ASTM D 4894 Type IV, Grade 2 classification
  • Produced by suspension polymerisation
  • Good mould filling behaviour
  • Very good free-flowing properties
  • Good mechanical properties
  • Very good surface quality of isostatically moulded articles
  • Excellent chemical inertness
  • Low friction behaviour
  • Good flame retardance
  • Exceptional temperature resistance

  • Typical Properties:

    PTFE moulding powder with very good free-flowing and feeding properties consisting of relatively large particles with high bulk density.

    This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Bulk density

    23.0 °C

    0.84 g/cm³

    Show Material materials with Bulk density of 0.84 g/cm³

    DIN EN ISO 60

    Density

    23.0 °C

    2.15 g/cm³

    Show Material materials with Density of 2.15 g/cm³

    DIN EN ISO 12086

    Particle size

    450000 nm

    Show Material materials with Particle size of 450000 nm

    ISO 13320, average value

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.6 GPa

    Show Material materials with Elastic modulus of 0.6 GPa

    DIN EN ISO 527

    Elongation

    23.0 °C

    430 %

    Show Material materials with Elongation of 430 %

    DIN EN ISO 527-3, 0.2 mm film

    Hardness, Shore D

    23.0 °C

    56 [-]

    Show Material materials with Hardness, Shore D of 56 [-]

    DIN EN ISO 868

    Tensile strength

    23.0 °C

    36 MPa

    Show Material materials with Tensile strength of 36 MPa

    DIN EN ISO 527-3, 0.2 mm film

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    100.0 °C

    1.2E-4 1/K

    Show Material materials with Coefficient of thermal expansion of 1.2E-4 1/K

    DIN 53 752, from 30°C to the mentioned temperature

    200.0 °C

    1.4E-4 1/K

    Show Material materials with Coefficient of thermal expansion of 1.4E-4 1/K

    DIN 53 752, from 30°C to the mentioned temperature

    260.0 °C

    1.7E-4 1/K

    Show Material materials with Coefficient of thermal expansion of 1.7E-4 1/K

    DIN 53 752, from 30°C to the mentioned temperature

    Thermal conductivity

    23.0 °C

    0.22 W/(m·K)

    Show Material materials with Thermal conductivity of 0.22 W/(m·K)

    DIN 52612

    Flammability

    V-0 UL94

    Electrical

    PropertyTemperatureValueComment

    Dielectric strength

    23.0 °C

    60 kV/mm

    Show Material materials with Dielectric strength of 60 kV/mm

    DIN EN ISO 12086, 0.2 mm film

    Electrical resistivity

    23.0 °C

    1.00E+16 Ω·m

    Show Material materials with Electrical resistivity of 1.00E+16 Ω·m

    IEC 60093

    Surface resistivity

    23.0 °C

    1.00E+17 Ω/sq

    Show Material materials with Surface resistivity of 1.00E+17 Ω/sq

    IEC 60093

    Rheological Properties

    PropertyTemperatureValueComment

    Shrinkage

    23.0 °C

    2.7 %

    Show Material materials with Shrinkage of 2.7 %

    Internal Dyneon method, Cylinder 45 mm diameter

    Technological properties

    Property
    Application areas

    3MTM DyneonTM PTFE Granules TF 1641 is a free-flowing compression moulding powder for applications like sealings, shaped parts, isostatically moulded articles – e.g. lined pipes and valves – or small parts like valve seats.