Kynar Flex® 2850-07

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar Flex® 2850-07 resin is a moderate viscosity version of

Kynar Flex® 2850-00 resin in for ease of extrusion and co-extrusion. It has a UL RTI temperature rating of 140 degrees C.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.77 g/cm³

Show Supplier Material materials with Density of 1.77 g/cm³

ISO 1183

Water absorption

23.0 °C

0.03 %

Show Supplier Material materials with Water absorption of 0.03 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.3 GPa

Show Supplier Material materials with Elastic modulus of 1.3 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

11 %

Show Supplier Material materials with Elongation at yield of 11 %

ISO 527-1/-2

Yield strength

23.0 °C

40 MPa

Show Supplier Material materials with Yield strength of 40 MPa

ISO 527-1/-2

Impact strength, Charpy notched

No break @ 23°C, ISO 179/1eA

Thermal

PropertyTemperatureValueComment

Melting point

157 °C

Show Supplier Material materials with Melting point of 157 °C

ISO 11357-1/-3, 10°C/min

Relative temperature index, electrical

140 °C

Show Supplier Material materials with Relative temperature index, electrical of 140 °C

UL 746B

Relative temperature index, mechanical strength

140 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C

UL 746B

Specific heat capacity

23.0 °C

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA, 1% wt. loss

Flammability

At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available

Electrical

PropertyTemperatureValueComment

Dielectric constant, 100Hz

23.0 °C

6.85 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 6.85 [-]

IEC 60250

Dielectric strength

23.0 °C

1.4 kV/mm

Show Supplier Material materials with Dielectric strength of 1.4 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

1.2E-5 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 1.2E-5 [-]

IEC 60250

Volume resistivity

23.0 °C

2.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

IEC 60093

Technological properties

Property
Application areas

Main applications:

  • injection molded applications requiring the high chemical and temperature resistance properties of Kynar 2850-00 resin

    or

    Chemical Process Industry,Chemical Process Industry - Injection Molding,Foamed PVDF Cable Jacketing,Performance Wire,Underground Fuel Containment