Elongation A11.3: 4 - 6 %

Quick Comparison

Wrought Copper Pure / Low Alloyed Copper

EN 12164 Grade CuSP R250

Wrought Copper Pure / Low Alloyed Copper

EN 12164 Grade CuTeP R250

Wrought Copper Brass Yellow Brass

EN 12163 Grade CuZn20 R450

Wrought Copper Brass Yellow Brass

EN 12166 Grade CuZn36 R460

Wrought Copper Brass Yellow Brass

EN 12168 Grade CuZn40 R500

Wrought Copper Brass Yellow Brass

EN 1652 Grade CuZn36 R550

Wrought Copper Brass Yellow Brass

EN 12166 Grade CuZn10 R440

Wrought Copper High Copper Alloy

EN 12164 Grade CuPb1P R250

Wrought Copper High Copper Alloy

EN 12163 Grade CuCo2Be R730

Wrought Copper High Copper Alloy

EN 12163 Grade CuCo2Be R680

Wrought Copper Bronze Silicon Bronze

EN 12163 Grade CuNi2Si R640
Página 1 de 3