Elongación A5 transversal: 10 - 14 %

Quick Comparison

Acero bajo en carbono

JIS G3444 Grade STK500

Acero de alto carbono

JIS G3201 Grade SF590B

Acero de alto carbono

JIS G3201 Grade SF640B

Acero inoxidable dúplex

JIS G3468 Grade SUS329J1TPY

Chromium Molybdenum Steel

JIS G3221 Grade SFCM590S

Chromium Molybdenum Steel

JIS G3221 Grade SFCM640S

Chromium Molybdenum Steel

JIS G3221 Grade SFCM690S

Chromium Molybdenum Steel

JIS G3221 Grade SFCM740S

Chromium Molybdenum Steel

JIS G3221 Grade SFCM780S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM690S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM740S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM780S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM830S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM880S

Nickel Chromium Molybdenum Steel

JIS G3222 Grade SFNCM980S

Chromium Molybdenum Steel

JIS G3221 Grade SFCM590D

Chromium Molybdenum Steel

JIS G3221 Grade SFCM640D

Chromium Molybdenum Steel

JIS G3221 Grade SFCM690D
Página 1 de 3