JIS G3201 Grade SF640B

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for High Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for High Carbon Steel

Elongation A5

23.0 °C

15 - 16 %

Show Material materials with Elongation A5 of 15 - 16 %

Elongation A5, transverse

23.0 °C

10 - 11 %

Show Material materials with Elongation A5, transverse of 10 - 11 %

Hardness, Brinell

23.0 °C

183 [-]

Show Material materials with Hardness, Brinell of 183 [-]

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for High Carbon Steel

Reduction of area

23.0 °C

35 - 40 %

Show Material materials with Reduction of area of 35 - 40 %

Reduction of area, transverse

23.0 °C

28 - 32 %

Show Material materials with Reduction of area, transverse of 28 - 32 %

Shear modulus

23.0 °C

81 GPa

Show Material materials with Shear modulus of 81 GPa

Typical for High Carbon Steel

Tensile strength

23.0 °C

640 - 780 MPa

Show Material materials with Tensile strength of 640 - 780 MPa

Yield strength

23.0 °C

345 - 390 MPa

Show Material materials with Yield strength of 345 - 390 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K

Typical for High Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1289 - 1478 °C

Show Material materials with Melting point of 1289 - 1478 °C

Typical for High Carbon Steel

Specific heat capacity

23.0 °C

486 J/(kg·K)

Show Material materials with Specific heat capacity of 486 J/(kg·K)

Typical for High Carbon Steel

Thermal conductivity

23.0 °C

36 W/(m·K)

Show Material materials with Thermal conductivity of 36 W/(m·K)

Typical for High Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel