JIS G3201 Grade SF590A annealed, normalized or normalized and tempered

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for High Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for High Carbon Steel

Elongation A5

20.0 °C

18 %

Show Material materials with Elongation A5 of 18 %

Elongation A5, transverse

20.0 °C

14 %

Show Material materials with Elongation A5, transverse of 14 %

Hardness, Brinell

20.0 °C

167 [-]

Show Material materials with Hardness, Brinell of 167 [-]

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for High Carbon Steel

Reduction of area

20.0 °C

35 %

Show Material materials with Reduction of area of 35 %

Reduction of area, transverse

20.0 °C

26 %

Show Material materials with Reduction of area, transverse of 26 %

Shear modulus

20.0 °C

75 - 80 GPa

Show Material materials with Shear modulus of 75 - 80 GPa

Typical for Carbon Steel

Tensile strength

20.0 °C

590 - 690 MPa

Show Material materials with Tensile strength of 590 - 690 MPa

Yield strength

20.0 °C

295 MPa

Show Material materials with Yield strength of 295 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K

Typical for High Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1289 - 1478 °C

Show Material materials with Melting point of 1289 - 1478 °C

Typical for High Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

20.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Chemical properties

PropertyValue

Carbon

0.6 %

Show Material materials with Carbon of 0.6 %

Iron

97.63 - 99.55 %

Show Material materials with Iron of 97.63 - 99.55 %

Manganese

0.3 - 1.2 %

Show Material materials with Manganese of 0.3 - 1.2 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.5 %

Show Material materials with Silicon of 0.15 - 0.5 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

Technological properties

Property
Processing history

annealed, normalized or normalized and tempered