Resistencia a la flexión: 14 MPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2750-01

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Superflex® 2500-20

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2950-05

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Superflex® 2500-25

Suministrada por:

Arkema: High Performance Polymers

Copoliéster termoplástico

HERAFLEX E MTE6005TK 100 NT

Suministrada por:

RadiciGroup High Performance Polymers

Termoplástico

Biopolymer CR1 1013

Silicato de aluminio

Pyrophyllite not heat treated