Description

An economical low ash material with excellent thermal shock resistance, GRAFSTARTM PJP graphite is well suited for the fine machining detail required in molds for casting metal shapes.

This material data has been provided by Advanced Graphite Materials.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.63 g/cm³

Show Supplier Material materials with Density of 1.63 g/cm³

Particle size range

0.76 µm

Show Supplier Material materials with Particle size range of 0.76 µm

Particle size

max.

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

34 MPa

Show Supplier Material materials with Compressive strength of 34 MPa

Elastic modulus

23.0 °C

6.9 GPa

Show Supplier Material materials with Elastic modulus of 6.9 GPa

Flexural strength

23.0 °C

14 MPa

Show Supplier Material materials with Flexural strength of 14 MPa

Tensile strength

23.0 °C

9 MPa

Show Supplier Material materials with Tensile strength of 9 MPa

Thermal

PropertyTemperatureValue

Ash content

23.0 °C

0.12 %

Show Supplier Material materials with Ash content of 0.12 %

Thermal conductivity, in-plane

23.0 °C

130 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 130 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

9.3E-6 Ω·m

Show Supplier Material materials with Electrical resistivity of 9.3E-6 Ω·m

Technological properties

Property
Application areas

Rail wheel molds