General
Property | Value | Testing Standard |
---|---|---|
Density | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.3 GPa Show Supplier Material materials with Elastic modulus of 0.3 GPa | ISO 527-2/1A | 1mm/min | |
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 33 % Show Supplier Material materials with Elongation at yield of 33 % | ISO 527-2/1A | 50mm/min | |
Flexural modulus | 0.27 GPa Show Supplier Material materials with Flexural modulus of 0.27 GPa | ISO 178 | 2mm/min | |
Flexural strength | 14 MPa Show Supplier Material materials with Flexural strength of 14 MPa | ISO 178 | 2mm/min | |
Hardness, Shore D | 52 [-] Show Supplier Material materials with Hardness, Shore D of 52 [-] | ISO 7619-1 | 15s | |
60 [-] Show Supplier Material materials with Hardness, Shore D of 60 [-] | ISO 7619-1 | inst. | ||
Impact strength, Charpy notched | -30 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | ISO 179/1eA | No Break at 23°C |
Impact strength, Charpy unnotched | No Break at 23°C | ISO 179/1eU | ||
Modulus at 10% elongation | 0.015 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.015 GPa | ISO 527-2/1A | ||
Modulus at 100% elongation | 0.018 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.018 GPa | ISO 527-2/1A | ||
Modulus at 300% elongation | 0.02 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.02 GPa | ISO 527-2/1A | ||
Tensile strength | 30 MPa Show Supplier Material materials with Tensile strength of 30 MPa | ISO 527-2/1A | 5mm/min | |
Yield strength | 20 MPa Show Supplier Material materials with Yield strength of 20 MPa | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 210 °C Show Supplier Material materials with Melting point of 210 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 5 g/10min Show Supplier Material materials with Melt mass-flow rate of 5 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Profile Extrusion,Other Extrusion |