White Cast Iron
EN 12513 Grade G-X 300 CrNiSi 9 5 2White Cast Iron
EN 12513 Grade G-X 330 NiCr 4 2White Cast Iron
EN 12513 Grade G-X 260 NiCr 4 2Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1400-1 cast conditionNickel Chromium Molybdenum Steel
ASTM A540 Grade B23 Class 1Acero inoxidable endurecido por precipitación
ASTM A564 Grade S45503 H900Acero inoxidable endurecido por precipitación
ASTM A564 Grade S46500 H950Nickel Chromium Molybdenum Steel
JIS G4108 Grade SNB23-1Acero inoxidable endurecido por precipitación
ASTM A705 Grade S45503 Age-Hardening H900Acero inoxidable endurecido por precipitación
ASTM A705 Grade XM-16 Age-Hardening H900Acero inoxidable endurecido por precipitación
ASTM A693 Grade 630 Precipitation hardened at 482 °CAcero inoxidable endurecido por precipitación
ASTM A564 Grade XM-16 H900Hierro fundido
ASTM A897 Class 3 AustemperedHierro fundido
ASTM A897 Class 4 AustemperedHierro fundido
ASTM A897 Class 5 Austempered