Dureza Rockwell B: 50 - 66 [-]

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TB00

Wrought Copper High Copper Alloy

ASTM B9 Grade C17510 TB00

Wrought Copper High Copper Alloy

ASTM B570 Grade C17000 TD01

Acero bajo en carbono

ASTM A109 Grade No. 5 Dead-Soft

Acero bajo en carbono

ASTM A513 Grade 1008 Sink-Drawn

Acero bajo en carbono

ASTM A513 Grade 1010 Normalized

Acero bajo en carbono

ASTM A513 Grade 1015 As-Welded

Acero bajo en carbono

ASTM A513 Grade 1020 As-Welded

Acero bajo en carbono

ASTM A519 Grade 1020 Normalized

Acero bajo en carbono

ASTM A519 Grade 1025 Normalized

Acero bajo en carbono

ASTM A513 Grade 1021 As-Welded

Acero bajo en carbono

ASTM A513 Grade 1025 As-Welded

Acero bajo en carbono

ASTM A513 Grade 1008 Normalized

Acero bajo en carbono

ASTM A513 Grade 1010 As-Welded
Página 1 de 12