Acero bajo en carbono
EN 10132-4 Grade C125S quenched and tempered (+QT)Acero de alto carbono
EN 10132-4 Grade C75S Quenched and TemperedAcero de alto carbono
EN 10132-4 Grade C100S quenched and tempered (+QT)Acero de alto carbono
EN 10132-4 Grade C85S quenched and tempered (+QT)Medium Carbon Steel
EN 10132-4 Grade C90S quenched and tempered (+QT)Medium Carbon Steel
EN 10132-3 Grade C50E quenched (+Q)Acero para herramientas y maquinaria
EN 10132-4 Grade 102Cr6 quenched and tempered (+QT)Acero para herramientas y maquinaria
EN 10132-4 Grade 80CrV2 quenched and tempered (+QT)White Cast Iron
EN 12513 Grade G-X 300 CrNiSi 9 5 2White Cast Iron
EN 12513 Grade G-X 330 NiCr 4 2Acero para herramientas y maquinaria
EN 10132-4 Grade 50CrV4 cold rolled, quenched and tempered (+C+QT)Chromium Vanadium Steel
EN 10132-4 Grade 51CrV4 quenched and tempered (+QT)Acero de alto carbono
EN 10132-4 Grade Ck85 cold rolled, quenched and tempered (+C+QT)Silicon Manganese Steel
EN 10132-4 Grade 67SiCr5 cold rolled, quenched and tempered (+C+QT)Medium Carbon Steel
EN 10083-2 Grade C45 quenched (+Q)White Cast Iron
EN 12513 Grade G-X 260 NiCr 4 2Silicon Manganese Steel
EN 10132-4 Grade 71Si7 cold rolled, quenched and tempered (+C+QT)Silicato de aluminio
General Aluminosilicate GlassAcero de alto carbono
JIS G4802 Grade CS85 quenched and temperedAcero de alto carbono
JIS G4802 Grade CS95 quenched and tempered