Resistencia al choque, ensayo Charpy entallado: 15 - 21 kJ/m²

Quick Comparison

Policarbonato (PC)

LEXAN™ Copolymer HPH4504H - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HPH4504H - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HPH4504H - Europe

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE250F9

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® 46HF5050

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6-FC

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G43L NC010

Polyamide 66 (PA66)

Zytel® 70G35HSL NC010

Policarbonato (PC)

LEXAN™ Copolymer HPH4504 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HPH4504 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HPH4504 - Americas

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Policarbonato (PC)

LEXAN™ Copolymer SLX2432T - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX2432T - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX2432T - Americas

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW241F10

Suministrada por:

DSM Engineering Materials
Página 1 de 29