General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.62 g/cm³ Show Supplier Material materials with Density of 1.62 g/cm³ | dry | ISO 1183 | |
Limiting oxygen index | 22 % Show Supplier Material materials with Limiting oxygen index of 22 % | dry | ISO 4589-1/-2 | |
Moisture absorption | 1.85 % Show Supplier Material materials with Moisture absorption of 1.85 % | dry | Sim. to ISO 62 | |
Water absorption | 1.9 % Show Supplier Material materials with Water absorption of 1.9 % | dry | ISO 62 | at 23°C after 24h |
6.75 % Show Supplier Material materials with Water absorption of 6.75 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 16.5 GPa Show Supplier Material materials with Elastic modulus of 16.5 GPa | dry | ISO 527-1/-2 |
10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | conditioned | ISO 527-1/-2 | ||
16 GPa Show Supplier Material materials with Elastic modulus of 16 GPa | dry | ISO 527-1/-2 | ||
100 °C | 9.5 GPa Show Supplier Material materials with Elastic modulus of 9.5 GPa | dry | ISO 527-1/-2 | |
120 °C | 8.5 GPa Show Supplier Material materials with Elastic modulus of 8.5 GPa | dry | ISO 527-1/-2 | |
140 °C | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | dry | ISO 527-1/-2 | |
150 °C | 7.6 GPa Show Supplier Material materials with Elastic modulus of 7.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 7.2 GPa Show Supplier Material materials with Elastic modulus of 7.2 GPa | dry | ISO 527-1/-2 | |
180 °C | 6.6 GPa Show Supplier Material materials with Elastic modulus of 6.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 6 GPa Show Supplier Material materials with Elastic modulus of 6 GPa | dry | ISO 527-1/-2 | |
210 °C | 5.8 GPa Show Supplier Material materials with Elastic modulus of 5.8 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 2.3 % Show Supplier Material materials with Elongation of 2.3 % | dry | ISO 527-1/-2 |
2.7 % Show Supplier Material materials with Elongation of 2.7 % | dry | ISO 527-1/-2 | ||
5 % Show Supplier Material materials with Elongation of 5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 | |
140 °C | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 | |
150 °C | 5.5 % Show Supplier Material materials with Elongation of 5.5 % | dry | ISO 527-1/-2 | |
160 °C | 5.5 % Show Supplier Material materials with Elongation of 5.5 % | dry | ISO 527-1/-2 | |
180 °C | 5.5 % Show Supplier Material materials with Elongation of 5.5 % | dry | ISO 527-1/-2 | |
200 °C | 6 % Show Supplier Material materials with Elongation of 6 % | dry | ISO 527-1/-2 | |
210 °C | 0.006 % Show Supplier Material materials with Elongation of 0.006 % | dry | ISO 527-1/-2 | |
Flexural modulus | 9 GPa Show Supplier Material materials with Flexural modulus of 9 GPa | conditioned | ISO 178 | |
15 GPa Show Supplier Material materials with Flexural modulus of 15 GPa | dry | ISO 178 | ||
120 °C | 7.3 GPa Show Supplier Material materials with Flexural modulus of 7.3 GPa | dry | ISO 178 | |
160 °C | 6.5 GPa Show Supplier Material materials with Flexural modulus of 6.5 GPa | dry | ISO 178 | |
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |
380 MPa Show Supplier Material materials with Flexural yield strength of 380 MPa | dry | ISO 178 | ||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |
160 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 24 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU |
-30 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | -40 °C | 290 MPa Show Supplier Material materials with Tensile strength of 290 MPa | dry | ISO 527-1/-2 |
150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | conditioned | ISO 527-1/-2 | ||
250 MPa Show Supplier Material materials with Tensile strength of 250 MPa | dry | ISO 527-1/-2 | ||
100 °C | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | dry | ISO 527-1/-2 | |
120 °C | 140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | dry | ISO 527-1/-2 | |
140 °C | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | dry | ISO 527-1/-2 | |
150 °C | 125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | dry | ISO 527-1/-2 | |
160 °C | 120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | dry | ISO 527-1/-2 | |
180 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 | |
200 °C | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-1/-2 | |
210 °C | 95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 1.39e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.39e-07 mm²/s | dry | - | |||
Vicat softening temperature | 290 °C Show Supplier Material materials with Vicat softening temperature of 290 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 300 V Show Supplier Material materials with Comparative tracking index of 300 V | dry | IEC 60112 | |
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.3 [-] Show Supplier Material materials with Dielectric constant of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.7 [-] Show Supplier Material materials with Dielectric constant of 4.7 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
16 [-] Show Supplier Material materials with Dielectric constant of 16 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 70 [-] Show Supplier Material materials with Dissipation factor of 70 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Dissipation factor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Dissipation factor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
6000 [-] Show Supplier Material materials with Dissipation factor of 6000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1420.0 g/cm³ Show Supplier Material materials with Density of melt of 1420.0 g/cm³ | dry | - | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Shrinkage of 0.9 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 1990 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1990 J/(kg·K) | dry | - | |
Spiral flow length | 70 | dry | - | 1.0 mm 800 bar |
80 | dry | - | 1.0 mm 900 bar | |
90 | dry | - | 1.0 mm 1000 bar | |
Thermal conductivity of melt | 0.391 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.391 W/(m·K) | dry | - | |
Viscosity number | 140 cm³/gr Show Supplier Material materials with Viscosity number of 140 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Off-road Vehicle Oil Pans and Reservoirs, MTF/DMF Components, Torque Convertor Components, Charge Air Cooler Caps, EPS Steering components: Gears, Flex couplers and Sensors, Wheel Speed Sensors, Endlaminates (electrical components), Gears, Timing drive systems, Electric parking brakes, Electric brake boosters, Electronic throttle control actuators, Exhaust gas recirculation actuators, Turbo actuators, Coolant valve actuators, Seat actuators, Mirror actuators, Trunk actuators, Door handle actuators, Sunroof actuators, Steering wheel adjusters | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |