Impact strength, Izod notched, ASTM: 748 J/m

Quick Comparison

Policarbonato (PC)

LEXAN™ FR Resin FXD153 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ FR Resin FXD153 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Resin EM1210