Impact strength, Izod notched, ASTM: 152 J/m

Quick Comparison

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL24

Suministrada por:

Sabic

Polieterimida (PEI)

PEI GF30 LFTG ®

Suministrada por:

Xiamen LFT composite plastic Co., Ltd.