PEI GF30 LFTG ®

Alternative and trade names
LFT-G® PEI-NANG-LGF30, PEI-LGF30
Want to keep this datasheet? Save it now in your required format

Description

Polyetherimide (PEI) reionforced with 30% long glass fiber.

This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Supplier Material materials with Density of 1.42 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

20.15 GPa

Show Supplier Material materials with Elastic modulus of 20.15 GPa

ASTM D638

Elongation

23.0 °C

1 - 2 %

Show Supplier Material materials with Elongation of 1 - 2 %

ASTM D638

Flexural modulus

23.0 °C

19.85 GPa

Show Supplier Material materials with Flexural modulus of 19.85 GPa

ASTM D790

Flexural strength

23.0 °C

275 MPa

Show Supplier Material materials with Flexural strength of 275 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

152 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 152 J/m

ASTM D256

Impact strength, Izod unnotched, ASTM

23.0 °C

530 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 530 J/m

ASTM D4812

Tensile strength

23.0 °C

205 MPa

Show Supplier Material materials with Tensile strength of 205 MPa

ASTM D638

Thermal

PropertyValue

Flammability

HB ASTM D635, for 1.5mm

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

100 - 10000 Ω/sq

Show Supplier Material materials with Surface resistivity of 100 - 10000 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.1 - 0.3 %

Show Supplier Material materials with Shrinkage of 0.1 - 0.3 %

ASTM D955, (1/8 in (3.2 mm)section)

Technological properties

Property
Color

Natural, and custom colors

Fillers

30% Long Glass Fiber

Processing methods

Injection Moulding. Injection Pressure 80 - 125 MPa, Melt Temperature 320 - 350 °C, Mould temperature 120 - 175 °C, Pre-drying 3 hrs @ 120 °C, Moisture Content 0.05%