Impact strength, Izod notched, ASTM: 52 J/m

Quick Comparison

Tereftalato de polibutileno (PBT)

VALOX™ FR Resins 771

Éter de polifenileno (PPE)

NORYL™ Resin RN0612 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DX09301C

Suministrada por:

Sabic

Éter de polifenileno (PPE)

LNP™ LUBRICOMP™ Compound ZX07421

Suministrada por:

Sabic

Polyamide 46 (PA46)

LNP™ LUBRICOMP™ Compound 9X06483

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

VALOX™ FR Resins V3504

Polipropileno

LNP™ THERMOCOMP™ Compound MFB22S

Suministrada por:

Sabic

Mezcla de polímeros

CYCOLOY™ FR Resins CM6220

Policarbonato (PC)

LNP™ STAT-KON™ Compound DE0069F - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DE0069F - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

LNP™ THERMOCOMP™ Compound EX93452 - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

LNP™ THERMOCOMP™ Compound EX93452 - Asia

Suministrada por:

Sabic