Bronce fosforado
UNS C51900 R350Bronce fosforado
UNS C51900 R420Bronce fosforado
UNS C51900 R500Bronce fosforado
UNS C51900 R560Bronce fosforado
UNS C51900 R640Bronce fosforado
UNS C51900 R720Bronce fosforado
UNS C51900 R850Zinc Aluminium
EN 12844 Grade ZP27Zinc Aluminium
EN 12844 Grade ZP8Zinc Aluminium
EN 12844 Grade ZP12Wrought Copper High Copper Alloy
CuCrZr Chromium Zirconium Copper HardSuministrada por:
Salomon's MetalenWrought Copper High Copper Alloy
CuCrZr Chromium Zirconium Copper SoftSuministrada por:
Salomon's Metalen