CuZn40 Hard

Alternative and trade names
Muntz Metal
Want to keep this datasheet? Save it now in your required format

Description

CuZn40 is a brass which is sometimes referred to as Muntz Metal. It shows antimicrobial properties according to CDA.

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Supplier Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

102 GPa

Show Supplier Material materials with Elastic modulus of 102 GPa

Elongation A5

23.0 °C

12 %

Show Supplier Material materials with Elongation A5 of 12 %

Hardness, Brinell

23.0 °C

130 [-]

Show Supplier Material materials with Hardness, Brinell of 130 [-]

Tensile strength

23.0 °C

470 MPa

Show Supplier Material materials with Tensile strength of 470 MPa

Yield strength Rp0.2

23.0 °C

390 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 390 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2.03E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.03E-5 1/K

Thermal conductivity

23.0 °C

117 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 117 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

1.50E+7 S/m

Show Supplier Material materials with Electrical conductivity of 1.50E+7 S/m

Chemical properties

PropertyValue

Copper

59 - 63 %

Show Supplier Material materials with Copper of 59 - 63 %

Iron

0 - 0.07 %

Show Supplier Material materials with Iron of 0 - 0.07 %

Lead

0 - 0.3 %

Show Supplier Material materials with Lead of 0 - 0.3 %

Other

0 - 0.3 %

Show Supplier Material materials with Other of 0 - 0.3 %

Zinc

36.3 - 41 %

Show Supplier Material materials with Zinc of 36.3 - 41 %