Leaded Brass
EN 12163 Grade CuZn35Ni3Mn2AlPb R490Leaded Brass
EN 1652 Grade CuZn37Pb0.5 R290Leaded Brass
EN 1652 Grade CuZn37Pb0.5 R370Leaded Brass
EN 1652 Grade CuZn37Pb0.5 R440Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 R460Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 R540Leaded Brass
EN 12163 Grade CuZn35Ni3Mn2AlPb H120Leaded Brass
EN 1652 Grade CuZn37Pb0.5 R540Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 H110Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 H150Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 H105Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 H125Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 R420Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 R470Leaded Brass
EN 1652 Grade CuZn37Pb0.5 H060Leaded Brass
EN 1652 Grade CuZn37Pb0.5 H110Leaded Brass
EN 1652 Grade CuZn37Pb0.5 H140Leaded Brass
EN 1652 Grade CuZn37Pb0.5 H170