Specific heat capacity melt: 1800 J/(kg·K)

Quick Comparison

Copoliéster termoplástico

Arnitel® EM460

Suministrada por:

DSM Engineering Materials

Copoliéster termoplástico

Arnitel® EM460-08

Suministrada por:

DSM Engineering Materials

Copoliéster termoplástico

Arnitel® EM460/U

Suministrada por:

DSM Engineering Materials