General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.15 g/cm³ Show Supplier Material materials with Density of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Water absorption | 0.7 % Show Supplier Material materials with Water absorption of 0.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.09 GPa Show Supplier Material materials with Elastic modulus of 0.09 GPa | dry | ISO 527-1/-2 | |
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | |
700 % Show Supplier Material materials with Elongation of 700 % | dry | ISO 527-1/-2 | ||
850 % Show Supplier Material materials with Elongation of 850 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 45 % Show Supplier Material materials with Elongation at yield of 45 % | dry | ISO 527-1/-2 | |
Flexural modulus | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | dry | ISO 178 | |
Hardness, Shore D | 43 [-] Show Supplier Material materials with Hardness, Shore D of 43 [-] | dry | ISO 868 | 3s |
Tear strength | 119 kN/m Show Supplier Material materials with Tear strength of 119 kN/m | dry | ISO 34-1; Method B | |
120 kN/m Show Supplier Material materials with Tear strength of 120 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 20 MPa Show Supplier Material materials with Tensile strength of 20 MPa | dry | ISO 527-1/-2 | Normal |
23 MPa Show Supplier Material materials with Tensile strength of 23 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.6e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.6e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Melting point | 189 °C Show Supplier Material materials with Melting point of 189 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | |
Thermal diffusivity | 5.99e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 5.99e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
Dissipation factor | 350 [-] Show Supplier Material materials with Dissipation factor of 350 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 928 g/cm³ Show Supplier Material materials with Density of melt of 928 g/cm³ | dry | - | ||
Melt volume-flow rate | 230 °C | 46 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 46 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.25 % Show Supplier Material materials with Shrinkage of 1.25 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1800 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1800 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties