Estaño: 6.5 - 7.5 %

Quick Comparison

Bronce fosforado

UNS C51900 R350

Bronce fosforado

UNS C51900 R420

Bronce fosforado

UNS C51900 R500

Bronce fosforado

UNS C51900 R560

Bronce fosforado

UNS C51900 R640

Bronce fosforado

UNS C51900 R720

Bronce fosforado

UNS C51900 R850

Bronce fosforado

JIS C5210HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM00 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM02 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM04 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM06 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM08 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TB00 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD01 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD02 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD04 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TB00 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD01 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD04 Strip (C72700)

Suministrada por:

Materion Brush GmbH
Página 1 de 20