General
Property | Value |
---|---|
Relative density | 8.8 [-] Show Supplier Material materials with Relative density of 8.8 [-] |
Mechanical
Property | Value | Comment |
---|---|---|
Bendability 90°, bw | 0 [-] Show Supplier Material materials with Bendability 90°, bw of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Bendability 90°, bw of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Bendability 90°, bw of 0 [-] | SH Temper | |
2 [-] Show Supplier Material materials with Bendability 90°, bw of 2 [-] | ESH Temper | |
4 [-] Show Supplier Material materials with Bendability 90°, bw of 4 [-] | XSH Temper | |
Bendability 90°, gw | 0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | SH Temper | |
0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | ESH Temper | |
0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | XSH Temper | |
Elastic modulus | 110 GPa Show Supplier Material materials with Elastic modulus of 110 GPa | |
Elongation | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | XSH Temper |
9.3 % Show Supplier Material materials with Elongation of 9.3 % | ESH Temper | |
13.3 % Show Supplier Material materials with Elongation of 13.3 % | SH Temper | |
23.2 % Show Supplier Material materials with Elongation of 23.2 % | EH Temper | |
35.3 % Show Supplier Material materials with Elongation of 35.3 % | H Temper | |
Flexural modulus | 100 GPa Show Supplier Material materials with Flexural modulus of 100 GPa | |
Hardness, Vickers | 197 [-] Show Supplier Material materials with Hardness, Vickers of 197 [-] | H Temper |
229 [-] Show Supplier Material materials with Hardness, Vickers of 229 [-] | EH Temper | |
242 [-] Show Supplier Material materials with Hardness, Vickers of 242 [-] | SH Temper | |
258 [-] Show Supplier Material materials with Hardness, Vickers of 258 [-] | ESH Temper | |
285 [-] Show Supplier Material materials with Hardness, Vickers of 285 [-] | XSH Temper | |
Tensile strength | 616 MPa Show Supplier Material materials with Tensile strength of 616 MPa | H Temper |
721 MPa Show Supplier Material materials with Tensile strength of 721 MPa | EH Temper | |
778 MPa Show Supplier Material materials with Tensile strength of 778 MPa | SH Temper | |
845 MPa Show Supplier Material materials with Tensile strength of 845 MPa | ESH Temper | |
979 MPa Show Supplier Material materials with Tensile strength of 979 MPa | XSH Temper | |
Yield strength | 469 MPa Show Supplier Material materials with Yield strength of 469 MPa | H Temper | for spring material (Kb0.1) |
563 MPa Show Supplier Material materials with Yield strength of 563 MPa | EH Temper | for spring material (Kb0.1) | |
569 MPa Show Supplier Material materials with Yield strength of 569 MPa | H Temper, RP02 | |
632 MPa Show Supplier Material materials with Yield strength of 632 MPa | SH Temper | for spring material (Kb0.1) | |
648 MPa Show Supplier Material materials with Yield strength of 648 MPa | ESH Temper | for spring material (Kb0.1) | |
694 MPa Show Supplier Material materials with Yield strength of 694 MPa | EH Temper, RP02 | |
706 MPa Show Supplier Material materials with Yield strength of 706 MPa | XSH Temper | for spring material (Kb0.1) | |
773 MPa Show Supplier Material materials with Yield strength of 773 MPa | SH Temper, RP02 | |
834 MPa Show Supplier Material materials with Yield strength of 834 MPa | ESH Temper, RP02 | |
968 MPa Show Supplier Material materials with Yield strength of 968 MPa | XSH Temper, RP02 |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 1.82e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.82e-05 1/K |
Melting point | 880 - 1020 °C Show Supplier Material materials with Melting point of 880 - 1020 °C |
Specific heat capacity | 377 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 377 J/(kg·K) |
Thermal conductivity | 63 W/(m·K) Show Supplier Material materials with Thermal conductivity of 63 W/(m·K) |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 12 % IACS Show Supplier Material materials with Specific Electrical conductivity of 12 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Iron | 0.01 % Show Supplier Material materials with Iron of 0.01 % | max. |
Lead | 0.01 % Show Supplier Material materials with Lead of 0.01 % | max. |
Other | 99.8 % Show Supplier Material materials with Other of 99.8 % | min. | Cu+Sn+P |
Phosphorus | 0.03 - 0.2 % Show Supplier Material materials with Phosphorus of 0.03 - 0.2 % | |
Tin | 7 - 9 % Show Supplier Material materials with Tin of 7 - 9 % | |
Zinc | 0.01 % Show Supplier Material materials with Zinc of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |