Viscosity number: 196 cm³/gr

Quick Comparison

Polyamide 6 (PA6)

Akulon® F130-C1

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F130-C2

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F130

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F130-C3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F130-E6 (F-X9307)

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F130-C

Suministrada por:

DSM Engineering Materials