Acero inoxidable austenítico
EN 10028-7 Grade X8NiCrAlTi32-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X8NiCrAlTi32-21 solution annealed (+AT)Acero inoxidable austenítico
DIN 17445 Grade G-X5CrNiNb18-9 quenched (+Q)Acero inoxidable austenítico
DIN 17460 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10213-4 Grade GX5CrNiNb19-11 solution heat-treated and quenchedTin Brass
EN 12451 Grade CuZn28Sn1As R320Acero inoxidable austenítico
EN 10213-4 Grade GX2CrNi19-11 solution heat-treated and quenchedTin Brass
EN 12452 Grade CuZn28Sn1As R320