DIN 17445 Grade G-X5CrNiNb18-9 quenched (+Q)

Want to keep this datasheet? Save it now in your required format

Description

G-X 5 CrNiNb 18 9, for casting parts in the food processing industry, photo industry, soap producing-, textile and paper industry, salpeter acid industry, ic resistant

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.9 g/cm³

Show Material materials with Density of 7.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Elongation

20.0 °C

20 %

Show Material materials with Elongation of 20 %

Hardness, Brinell

20.0 °C

130 - 200 [-]

Show Material materials with Hardness, Brinell of 130 - 200 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

20.0 °C

440 - 640 MPa

Show Material materials with Tensile strength of 440 - 640 MPa

Yield strength Rp0.2

20.0 °C

175 MPa

Show Material materials with Yield strength Rp0.2 of 175 MPa

100.0 °C

150 MPa

Show Material materials with Yield strength Rp0.2 of 150 MPa

150.0 °C

135 MPa

Show Material materials with Yield strength Rp0.2 of 135 MPa

200.0 °C

130 MPa

Show Material materials with Yield strength Rp0.2 of 130 MPa

250.0 °C

125 MPa

Show Material materials with Yield strength Rp0.2 of 125 MPa

300.0 °C

120 MPa

Show Material materials with Yield strength Rp0.2 of 120 MPa

350.0 °C

115 MPa

Show Material materials with Yield strength Rp0.2 of 115 MPa

400.0 °C

110 MPa

Show Material materials with Yield strength Rp0.2 of 110 MPa

450.0 °C

105 MPa

Show Material materials with Yield strength Rp0.2 of 105 MPa

500.0 °C

100 MPa

Show Material materials with Yield strength Rp0.2 of 100 MPa

550.0 °C

90 MPa

Show Material materials with Yield strength Rp0.2 of 90 MPa

Yield strength Rp1.0

20.0 °C

200 MPa

Show Material materials with Yield strength Rp1.0 of 200 MPa

100.0 °C

175 MPa

Show Material materials with Yield strength Rp1.0 of 175 MPa

150.0 °C

160 MPa

Show Material materials with Yield strength Rp1.0 of 160 MPa

200.0 °C

155 MPa

Show Material materials with Yield strength Rp1.0 of 155 MPa

250.0 °C

150 MPa

Show Material materials with Yield strength Rp1.0 of 150 MPa

300.0 °C

145 MPa

Show Material materials with Yield strength Rp1.0 of 145 MPa

350.0 °C

140 MPa

Show Material materials with Yield strength Rp1.0 of 140 MPa

400.0 °C

130 MPa

Show Material materials with Yield strength Rp1.0 of 130 MPa

450.0 °C

120 MPa

Show Material materials with Yield strength Rp1.0 of 120 MPa

500.0 °C

110 MPa

Show Material materials with Yield strength Rp1.0 of 110 MPa

550.0 °C

100 MPa

Show Material materials with Yield strength Rp1.0 of 100 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

200.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

300.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

400.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

500.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 550 °C

Show Material materials with Max service temperature, long of 0 - 550 °C

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

15 W/(m·K)

Show Material materials with Thermal conductivity of 15 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

5.5E-7 - 7.5E-7 Ω·m

Show Material materials with Electrical resistivity of 5.5E-7 - 7.5E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.06 %

Show Material materials with Carbon of 0.06 %

Chromium

18 - 20 %

Show Material materials with Chromium of 18 - 20 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Nickel

9 - 11 %

Show Material materials with Nickel of 9 - 11 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1.5 %

Show Material materials with Silicon of 1.5 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %