Acero bajo en carbono
DIN 1629 Grade St 44.0 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17200 Grade C22 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17243 Grade C22.8 normalized or normalized formed (+N)Acero bajo en carbono
EN 10277-5 Grade C22 cold drawn or turned and quenched and temperedAcero bajo en carbono
EN 10277-5 Grade Ck22 cold drawn or turned and quenched and temperedAcero bajo en carbono
EN 10216-2 Grade St 45.8 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17200 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10273 Grade P250GH normalized or normalized formed (+N)Acero bajo en carbono
EN 10132-3 Grade C22E soft annealed or soft annealed and skin passed (+A or +A+LC)Acero bajo en carbono
ISO 683-1 Grade C22E quenched and tempered (+QT)Acero bajo en carbono
EN 10297-1 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10297-1 Grade Ck22 quenched and tempered (+QT)Acero bajo en carbono
EN 10277-5 Grade C22 cold drawnAcero bajo en carbono
EN 10277-5 Grade C22 cold drawn or turned and normalizedAcero bajo en carbono
EN 10277-5 Grade Ck22 cold drawnAcero bajo en carbono
EN 10277-5 Grade Ck22 cold drawn or turned and normalizedAcero bajo en carbono
ISO 683-1 Grade C22E normalized or normalized formed (+N)Acero bajo en carbono
BS 970-1 Grade 070M20 NormalizedAcero bajo en carbono
DIN 2391-2 Grade St 45 normalized or normalized formed (+N)