Acero inoxidable austenítico
EN 10270-3 Grade X10CrNi18-8 cold drawnAcero inoxidable austenítico
EN 10088-1 Grade X10CrNi18-8 strain-hardened (+C800)Acero inoxidable austenítico
JIS G4303 Grade SUS303Se solution treatedAcero inoxidable austenítico
JIS G4306 Grade SUS302 hot-rolled, solution annealedAcero inoxidable austenítico
JIS G4307 Grade SUS302 cold-rolled, solution annealedAcero inoxidable austenítico
ASTM A240 Grade 302 Heat-TreatedAcero inoxidable austenítico
ASTM A511 Grade MT302 AnnealedAcero inoxidable austenítico
ASTM A554 Grade MT302Acero inoxidable austenítico
ASTM A666 Grade 302 AnnealedAcero inoxidable austenítico
ASTM A276 Grade 302 Annealed; Hot-FinishedAcero inoxidable austenítico
ASTM A276 Grade 302 Relatively severe Cold work; Cold-FinishedAcero inoxidable austenítico
ASTM A473 Grade 302 AnnealedAcero inoxidable austenítico
ASTM A479 Grade 302 AnnealedAcero inoxidable austenítico
ASTM A580 Grade 302 Condition A; Cold finishedAcero inoxidable austenítico
ASTM A666 Grade 302 Full HardAcero inoxidable austenítico
ASTM A666 Grade 302 1/4 HardAcero inoxidable austenítico
ASTM A666 Grade 302 1/8 HardAcero inoxidable austenítico
ASTM A666 Grade 302 1/16 Hard