ASTM A666 Grade 302 Annealed

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

7.9 - 8.2 g/cm³ at 20 °C

Typical for Austenitic Stainless Steel

Mechanical

Elastic modulus E

195 GPa at 20 °C

Typical for Austenitic Stainless Steel

Elongation A50 A50

40 % at 20 °C

Hardness, Brinell HB

201 [-] at 20 °C

Hardness, Rockwell B HRB

92 [-] at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Typical for Austenitic Stainless Steel

Tensile strength Rm

515 MPa at 20 °C

Yield strength YS

205 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.7E-5 - 1.9E-5 1/K at 20 °C

Typical for Austenitic Stainless Steel

Melting point Tm

1375 - 1450 °C

Typical for Austenitic Stainless Steel

Specific heat capacity cp

440 J/(kg·K) at 20 °C

Typical for Austenitic Stainless Steel

Thermal conductivity λ

11 - 21 W/(m·K) at 20 °C

Typical for Austenitic Stainless Steel

Electrical

Electrical resistivity ρel

8.5E-7 Ω·m at 20 °C

Typical for Austenitic Stainless Steel

Chemical properties

Element

Weight %

Comment

Cr

17 - 19 %

Ni

8 - 10 %

Mn

2 %

Si

0.75 %

C

0.15 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.